Sticking to Bullseye paper
Home › Forums › Glass Fusing › General Fusing Discussion › Help! Shelf paper sticking to glass! › Sticking to Bullseye paper
March 27, 2013 at 1:46 pm #12890
Participant
Hi,
I had that problem when I fired my new kiln for the first time. With further firings, the problem just went away. I was using Spectrum on Bullseye paper. I have no verifiable explanation but I do have a hypothesis : a new kiln might have a substance that burns out in the first firings, a substance that affects the non stickability of the paper.
Good luck!