sticking kiln wash
Home › Forums › Glass Fusing › General Fusing Discussion › Fusing Kokomo Glass › sticking kiln wash
November 17, 2009 at 8:53 pm #11431
Participant
If the kiln wash is sticking, you may be firing too high. What temps are you using and how long are you soaking a the top temperature?
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/