Stephen,
Thanks for the reply. Just fired 5 Red Stripe bottles @ 1350 …. 4 “labels” burned off, 1 was fine. I watched thru peep hole and it appeared that enamel started to burn off @ 1100. I agree with your comment about composistion of enamel. Do you think putting a coat of clear paint medium over the “label” would prevent burn off? I tried clear coat overglaze and this did not seem to help at all.
Thanks,
John
John Leutheuser