Sorry to hear that. If none
Home › Forums › Glass Fusing › General Fusing Discussion › Cracked Kiln Shelf › Sorry to hear that. If none
October 16, 2011 at 2:20 am #12255
Inactive
Sorry to hear that.
If none of the glass stuck to the shelf it was probably thermal shock.
What kind of kiln and what was the schedule?
Paul