Sorry about that. I guess that’s what happens when I read posts past my bedtime.
There is a technique where you place a piece of iridized glass on top of a stack of pieces and full fuse. The iridized coating can’t stretch so it crackles. Take a look at the last work on this page for an example: http://www.malinacipleu.com/fused-glass-bowls-and-trays.html