Some bottle glass had an

Home Forums Glass Fusing General Fusing Discussion pit holes in fused glass Some bottle glass had an

#11496
Anonymous
Inactive

Some bottle glass had an exceptionally high melting temp (compared to glass intended for fusing).

I recently tried to fuse some brown beer bottle pieces into a single “blank” — after 6 hours at the kilns top temperature of 1700° F I gave up.



Paul