My kiln (a Skutt Hot Start Pro) has several pre-programmed schedules. All of them start with the soak at 300F so I assumed that step is unique to the smooth operation of this particular kiln. So I just include that segment in any of the programs I write – I figure it can’t hurt anything…
Thanks for the input!