small 3/4 inch mold for jewelry
Home › Forums › Glass Fusing › General Fusing Discussion › small 3/4 inch mold for jewelry › small 3/4 inch mold for jewelry
March 11, 2010 at 3:47 pm #11566
Participant
Hi Pam,
I use frit with a mold like that; I haven’t tried putting in layers of glass circles to slump or larger scrap to melt together. With the frit, the bottom of the mold is the bottom of the cab. I fill the depressions with frit and sometimes add smaller scraps of dichroic, stringer, etc to the top of the “pile” and the cab rounds over pretty nicely during the fusing.
Sherrie
SherrieB