Slumping with “bottomless”
Home › Forums › Glass Fusing › General Fusing Discussion › Question about fusing and trying to make both sides shiny. › Slumping with “bottomless”
January 2, 2013 at 6:23 am #12785
Inactive
Slumping with “bottomless” molds (drop rings) will get you shiny on both sides. You can then cut off the rim for a more traditional bowl shape.
Paul