Just curious if anyone has tried this project in a Paragon II kiln? I followed the firing schedule, but my strips didn’t budge at all. I next tried Slumpy’s schedule for slumping, and the best I got was a 50 degree angle. I’m wondering if that’s good enough to proceed with the second slump for total foldover. Do I need to go with a higher temp, or longer hold at slumping temperature (or both) to get the strips to do more of a lean towards total foldover before the second step??