Silver reaction
Home › Forums › Glass Fusing › General Fusing Discussion › I am encasing silver and silver foil into 2 glasses and the silver comes out with gold color what I am doing wrong ? Thanks for › Silver reaction
May 3, 2015 at 5:44 pm #13527
Participant
I hope this is helpful, as I am only familiar with Bullseye glass.
Silver can cause a reaction when fired with sulfur/selenium-bearing glass. One of my favorites is their French Vanilla.
If you are using a clear glass, and if it is from Bullseye, it sounds as if you may be using the Silver to Gold in their Alchemy series.
Again, I hope this is helpful.