Short answer – no

#12899
Stephen Richard
Participant

But it is possible with a lot of work.  You have to abrade the unwanted pieces from the surface of the piece.  I have sandblasted off something that I absolutly had to save.

Mainly, it it just isn’t worth the effort, especially on a delicate tack fused piece.  Make another is my recommendation.

Stephen Richard

blogs at: http://www.verrier-glass.blogspot.com/ and  http://www.glasstips.blogspot.com/