Clay-king:

http://www.clay-king.com/kilnshelves.htm#shelves

 

Flipping the shelf is a good idea. Also, you might try firing on 1/8″ fiber blanket and see if that resolves the problem. The fiber blanket would let the air escape from under the piece — not a good long-term solution, however.

Dana

Jester’s Baubles Fused Glass Designs

http://www.jestersbaubles.com