Dear Barry:
Is anyone screenprinting directly onto glass?  I have sprinkled powdered enamels and inclusions, but would like to use screenprinting techniques.  Is there a binder that people have had some success in using to screenprint the powders?  I was thinking of watered down school glue, but if someone has used it and found it forms bubbles frequently or creates a dark “burn smear” then I’d just as soon not do that experiment.  Thanks for the posts.