Ih this case, size doesn’t matter ;).

It’s all about how the individual kiln, itself, fires. Top vs. side vs. top + side elements; hot spots; max rate of heating and cooling because of kiln size and construction, etc. I think you’ll just need to start playing and adjust if/when necessary.

I have a “small”, “medium”, and “large” kiln, and I pretty much use the same schedules for all three.

Dana W.

Jester’s Baubles Fused Glass Designs

http://www.jestersbaubles.com