sand paper
Home › Forums › Glass Fusing › General Fusing Discussion › Question about Kiln Liner Fusing Release Paper › sand paper
April 23, 2011 at 8:06 am #12054
Participant
You can use wet and dry sandpaper to remove the deposit and then fire.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/