My suggestion is to stop before the rubbing alcohol. It has additives that won’t do you glass any good. After the water and soap rinse thoroughly, then polish dry with un-printed paper towels or cloth towells that have had no fabric softer used with them at any time during washing and drying. The streaks are the bits of residue left by alcohol and or cloth.