rubber stamps
Home › Forums › Glass Fusing › General Fusing Discussion › Imaging with Rubber Stamps › rubber stamps
September 13, 2012 at 1:30 am #12683
Participant
Hi I haven’t done stamping, but I have done stencleing. When I do stencleing I dab my sponge on newspaper or napkins first before stencleing on glass, to get rid of extra moisture. For stamping I would mix glass powder with a little water to make a paste, then stamp on newspaper or napkins before stamping on glass.