January 29, 2012 at 9:41 am #11888
Participant
I just did a paperweight and a tray with rods, not sure what kind they had been sitting around the studio for a long time and we think they got might have been Bullseye, but it was beforeĀ I got there. I cut up pieces of transparent and filled up a done mold then added a alayer of opaqe, looked very nice.
The tray I just laid them out side by side and tack fused them twice, they are all just a little different in lenght and it looks really cool.