Refiring
Home › Forums › Glass Fusing › General Fusing Discussion › Surface pits › Refiring
December 7, 2011 at 10:46 pm #12334
Participant
“Which segment should be slower/lower?”
hard to say as no information on your firing schedule is available.
“Will refiring smooth out the surface?”
Possibly. It is also possible that you will reveal other bubbles.
Sharing some information about your firing schedules, your firing conditions, your layup, your kind of kiln (side or top fired for example), will help people give you appropriate advice. Was the information in the glass tips blog any use?
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/