Ready to fire shelf level

#12219
baxters
Participant

Please review my firing schedule:

200/1000/15-I want to go as slow as possible so it won’t break.

200/1250/30 to make suree all glass is at the same temp

300/1500/ 4 hours long hold to allow glass to move to same thickness

9999/900/2 hours

50/800/00 for a slow cool down

100/400/00

off

OR

200/500/00

250/1000/00

300/1500/4 hours

I’m still not sure if i should have a hold time 1250.

I’ve cleaned it, flipped it(placed top side on the shelf, and leveled the shelf . Ready to fire. I will to hear your comments on the schedule though!

Thanks again. And I am keeping a log. Susanne