Quick fire fusing
Home › Forums › Glass Fusing › General Fusing Discussion › Dichroic Firing Using a Quick Fire › Quick fire fusing
June 22, 2015 at 4:10 am #13121
Participant
I’ve used a quickfire for fusing jewelry and I lift the lid to check on the progress, once it’s fused to my liking, I just turn the kiln off, I vent after 5 minutes. I have never needed a controller (I don’t think they even make one) they heat up very fast, they cool down very fast.