Pot melts and pulling Vitrograph cane
Home › Forums › Glass Fusing › General Fusing Discussion › Projects gone Bad › Pot melts and pulling Vitrograph cane
April 4, 2014 at 3:17 am #13320
Participant
I use old projects for pot melts and pulling cane. Some glass can shift coe after several fusing so thats the only thing i can think of that could be a problem.