July 29, 2012 at 1:44 am #12607
Participant
I have had really good results using a clear piece of glass on my kiln shelf and it becomes part of the melt but works really well and no sticking problems because I use kiln paper under the glass. I actually use legs under stainless steel screen and get some really varied effects rather than the regular look of pot melts. Good luck