Polishing
Home › Forums › Glass Fusing › General Fusing Discussion › devitrification › Polishing
April 5, 2014 at 8:12 pm #13313
Participant
Unless the piece is flat, fire polishing, even to a matt finish will probably distort the piece as fire polishing occurs at ca. 740C and over.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/