September 7, 2008 at 7:06 am #10726
Participant
Here’s are two links I found when I was considering doing photo realistic decals. It sounds like you need special "ceramic toners" in an inkjet printer for color, or a toner with a high iron oxide content in a laser printer, to get it to work. Hope this helps.
Cerebus
http://www.glass-fusing-made-easy.com/fusing-photo-paper.html
http://www.dcphub.com/Process.htm
“You use a glass mirror to see your face; you use works of art to see your soul” -George Bernard Shaw