Peaked at near the end of
Home › Forums › Glass Fusing › General Fusing Discussion › First screen melt! › Peaked at near the end of
July 1, 2013 at 3:54 am #12992
Participant
Peaked at near the end of the hold at 1700. Man is that hot! Was wearing protective gloves and glasses but my forearms still got singed just opening the kiln. Even with glasses it was hard to tell how much glass had melted through. I know there was still glass dripping but there was also glass in the ring. I guess I’m going to have to wait until it cools to see if this worked or not.
I now have a new understanding of “white hot” …