I do not recomend trying to melt or slump a Patron bottle.  I have looked at many examples where others have tried and it just turns into a huge glob of glass.  Such a waste of a beautiful bottle.  I have seen a tutorial on YouTube on how to cut the bottle and make a bird feeder.  Very clever.  Hope that helps!