It is hard to give a fusing schedule when we don’t know what you did..but for 3 layers versus 2 you will need a higher temp and or, longer soak times. Try soaking for around 15-20 min at around 1000 f before going to the peak temp and if that is not enough then soak at the peak temp for 10 – 15 mins. Hope this helps… I have found patience is the hardest thing to learn when fusing. I don’t peek much anymore.
Pam