I too just had to try this. I used the fused pieces in a stained glass panel and have gotten numerous compliments. I just used glass powders in different shades of green with clear textured spectrum stained glass on top of the leaves. I love the texture the leaves left on the glass and the patterns turned out perfectly with no plant residue. I do plan to play around with this some more.