October 21, 2010 at 9:15 pm #11762
Participant
Far too hot – by about 100C. The best thing to do is to watch any new firing to determine the temperatures required. Probably nothing to be done about the over fired piece.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/