Needlepoints/spikes when slumping
Home › Forums › Glass Fusing › General Fusing Discussion › Needle points or spikes when Slumping › Needlepoints/spikes when slumping
February 13, 2014 at 12:34 am #13257
Participant
Dana W,
Thank you for your reply. It was suspect that the temp might be running too hot but was not confident about changing it. What temp is good for fire polish – mine is set around 1200 deg F. When I fire polished a piece I was quite surprised it relaxed as much as it did.
Again, thank you for your input……