My interpretation is 20
Home › Forums › Glass Fusing › General Fusing Discussion › Firing Schedule for a CEO 90 › My interpretation is 20
April 2, 2014 at 2:51 am #13316
Participant
My interpretation is 20 degrees to the target process temperature.
It would probably be wise to visit Bullseye’s web site and read their suggested firing schedules. From there, you should be able to figure it out.
Dana W.