June 13, 2017 at 7:27 pm #13705
Participant
I have found that I needed to make sure the glass was extremely clean, and that I had to leave the Etchall on longer than the instructions say. I believe I was leaving it on twice as long. I wash my glass with Dawn and hot water, air dry, then swipe it with rubbing alcohol just before etching. I hope that helps.