Mustafa,
You cannot use glass clay to make a clear project. Fusing the clay traps tiny air bubbles causing the clay to be opaque or, at very best, translucent.
I know a little(not much) about bronze clay, but I do know that it cannot be torch fired. It needs to be fired in a reducing environment. They fire it in a pan of charcoal to keep the oxygen out. out.
Barry Kaiser
Web Site http://www.kaiserglass.com