Participant
Moretti Rods
information from yglass.com.
Specifications: Coefficient of Expansion (C.O.E): 104x10C
Rods per pound:7-8 Rod
Length: Approx 39″ (1meter)
Rod Diameter:5-6mm
Strain Point: 840 Farenhiet 448C
Working Temprature: 1700 Farenhiet 926C
Annealing Range: 920-928 Farenheit 493 – 498C
Softening Point: 1050 Farenheit. 565C
This is for rods and does not give the full fuse temperature, but I would guess it would be 5-10C below S96.