January 20, 2009 at 5:46 am #11079
Participant
Maybe we are talking about different things. I purchased them from Delphiglass – they are very limited in color range – red, black, 2 blues, yellow, white, green … I think that’s it – don’t feel like jumping over to look. I forget what they cost – but they send you a TON of them – usually I’m disappointed with the quantity I get for the money – in this instance I was thinking – I’ll never use this stuff up in my lifetime, LOL Some of them are so threadlike (thin) they are really hard to pick up and place – and then drat they widen like a tick after you fire them sometimes.