Wash the mold thoroughly. Heat to about 500 degrees in the kiln or over, apply kiln wash. You may need to repeat a few times to get a nice coat of kiln wash. Many people use a spray bottle for the kiln wash, or you can brush it on but brushing is pretty messy.