Mixed glass
Home › Forums › Glass Fusing › General Fusing Discussion › Fusing Assorted Glass Shards › Mixed glass
January 30, 2012 at 8:49 am #12408
Participant
With the understanding that it could all crack at any time, you can take it to a tack fuse.
I have done a couple of things thes way, some bottles and two pieces of art glass, I cut and did any fire polishing that was nessecary and then did a low tack fuse, then with the art glass I slumped it into a sushi platter mold. As far as I know it is all still doing ok. It was done for a friend, the bottles had sentemnental value and she just loved the glass.
Good luck,
Jo