September 17, 2018 at 11:48 am #12544
Participant
Lynda M Keen I had the same problem the other day for the first time. I am new to a large microwave kilning too. The paper curled up around the edges of the rectangle, then it turned into an oval! I do start slowly usually at 40% to 50%. I think my problem is heating the glass too long. The large MK takes me about 15-17min. to complete.