I would not recommend getting a microwave kiln unless you don’t want to spend more.  You have to watch them very closely and after the first minute of firing, you have to fire only 30 seconds at a time.  You can use any kind of glass, just not mixed.  Also, you will probably only fire one piece at a time as there isn’t much space. 