I had a huge stash of mica left over from my paper and poly caly days.
I useda sticky pad and rubber stamp to grab the powders and hold them in place and then capped them with clear, came out amazing, some of the owders gave off lots of bbbles but it worked out really well and added to the design.
I have been working on my new class schedule and added a section for inclusions and my powders are going to be part of that class, will post pictures after they are done.