Janice,
If you were to use the same amount and thickness (not very realistic) of 96, it would be compatible with the 90. The reason that enamel paints are compatible with a wide variety of COEs is that the layer is thin.
Metal has one other problem that applied glass does not. That is it absorbs and dissapates heat much fast than glass. This can cause thermal shock if you push the envelope too much.
Barry Kaiser
Web Site http://www.kaiserglass.com