Making your own Frit
Home › Forums › Glass Fusing › General Fusing Discussion › Make your own frit › Making your own Frit
April 12, 2016 at 6:53 pm #13610
Participant
Just a Post Script on the above . Make sure the glass is really clean and free of oils dirt ect. Also Never use a plastic bucket.
MonaKeys