 think you hit it right on. I have a clam shell, 20″ shelf–i.e. top elements.

All the items are slumping more so in the back than the front. I don’t
know where to move the stuff so they will slump more evenly.

I guess it will be a lot of work (and glass) to figure out the correct
position as far as forward or back or if it is even possible with this
configuration.

Any more suggestions would be good.