Kiln Wash
Home › Forums › Glass Fusing › General Fusing Discussion › kiln wash › Kiln Wash
May 10, 2009 at 4:20 am #11291
Participant
Paul is correct. I do a lot of pot melts and that glass is melting at 1700 degrees for two hours. Very seldom do I have a problem with the melt actually sticking to the shelf. When I do I figure that it happened because I didn’t cover the shelf completely. I just sandblast it off and refuse, which I need to do anyway because of all the bubbles on the surface at that temp.