Jolinda and Don,

I’ll try  and answer both of your questions. First, the process of making a silk screened decal is probably far beyond where you want to go. The decals we are talking about here are only the sepia colored ones made on a laser printer. The full color decals involve silk screening colors onto the paper and then covering them with gelatin.

Don, I have to agree with you about the confusion on papers.  I originally bought a large supply of the decal paper from Beldecal because I use it in two of my classes.After looking at the site, I don’t know for sure which one I bought, but I think it is the regular clear laser paper. I would suggest you call them and ask.

 

Barry Kaiser