I’ve never heard of devit
Home › Forums › Glass Fusing › General Fusing Discussion › Devit problem in kiln › I’ve never heard of devit
October 14, 2010 at 4:37 pm #11746
Inactive
I’ve never heard of devit occuring differently in different parts of the kiln. In a larger kiln I can imagine a scenario – but not in a 14″ kiln.
I have a couple questions –
– what model kiln
– are you grinding the edges of your cabs?
– are you firing on shelf primer, shelf paper, ?
Thanks,
Paul
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com