I’ve had mixed results with
Home › Forums › Glass Fusing › General Fusing Discussion › Question about fusing and trying to make both sides shiny. › I’ve had mixed results with
January 11, 2013 at 12:52 am #12790
Inactive
I’ve had mixed results with borax. The directions for preparing it are on this site here:
https://fusedglass.wpengine.com/learn/recipes/devitrification_spray
I much prefer the commercial Super Spray and Bending Glaze products.
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com