I’ve gone as thin as about
Home › Forums › Glass Fusing › General Fusing Discussion › Pressed glass › I’ve gone as thin as about
February 20, 2013 at 5:34 pm #12850
Inactive
I’ve gone as thin as about 2mm. You need to have sufficient weight and proper spacers.